Por favor, use este identificador para citar o enlazar este ítem: http://ciateq.repositorioinstitucional.mx/jspui/handle/1020/397
Electrochemical performance of Fe40Al-X (X = Cr, Ti, Co, Ni) alloys exposed to artificial saliva
CINTHYA DINORAH ARRIETA GONZALEZ
ROBERTO ADEMAR RODRIGUEZ DIAZ
Jan Mayén Chaires
ROGEL FERNANDO RETES MANTILLA
MARIA TERESA TORRES MANCERA
LYA ADLIH OROS MENDEZ
HECTOR CRUZ-MEJIA
NESTOR STARLIN FLORES GARCIA
JESUS PORCAYO-CALDERON
Acceso Abierto
Atribución-NoComercial-CompartirIgual
https://doi.org/10.3390/ma13051095
1996-1944
https://www.mdpi.com/1996-1944/13/5/1095
Intermetallics
Artificial saliva
Electrochemical technics
Corrosion
Biomaterials
Fe-Al intermetallic compounds have been considered excellent candidates as alternative alloys for various applications in corrosive environments compared to other Fe-based alloys. Their excellent corrosion resistance is due to the development of an Al-based passive layer. The performance of the passive layer can be improved by adding a third alloy element. Therefore, in this study the electrochemical performance of the Fe40Al intermetallic alloy modified by the addition of a third alloy element (Cr, Ti, Co, Ni) is evaluated. The corrosion resistance of intermetallic alloys has been evaluated by electrochemical tests (potentiodynamic polarization curves, and measurements of open circuit potential, linear polarization and electrochemical impedance) in artificial saliva. The performance of intermetallic alloys was compared with that of Ti. The results obtained showed that the addition of Ni and Ti substantially improves the corrosion resistance of the base intermetallic. The corrosion resistance shown is comparable or greater than that shown by Ti. However, the addition of Co reduces the corrosion resistance of the base intermetallic.
Author contributions: Conceptualization, R.A.R.-D., M.T.T.-M. and H.C.-M.; Data curation, M.T.T.-M.; Formal analysis, J.M., L.A.O.-M. and H.C.-M.; Investigation, C.D.A.-G., R.A.R.-D., R.F.R.-M., L.A.O.-M., N.S.F.-G. and J.P.-C.; Methodology, C.D.A.-G., J.M., R.F.R.-M., M.T.T.-M., L.A.O.-M., H.C.-M., N.S.F.-G. and J.P.-C.; Project administration, R.A.R.-D., J.M., R.F.R.-M. and J.P.-C.; Supervision, N.S.F.-G.; Validation, J.P.-C; Writing—Original draft, C.D. A.-G., J.M. and J.P.-C.; Writing—Review & Editing, R.A.R.-D. and J.P.-C. All authors have read and agreed to the published version of the manuscript.
Funding: This research received no external funding.
Acknowledgments: The authors thank our aliation institutions for the facilities granted for carrying out this research work.
Conflicts of Interest: The authors declare no conflict of interest.
MDPI
2020
Artículo
Materials, vol. 13, no. 5, p. 1095-1100
Inglés
Público en general
Arrieta-Gonzalez, C.D.; Rodriguez-Diaz, R.A.; Mayen, J.; Retes-Mantilla, R.F.; Torres-Mancera, M.T.; Oros-Méndez, L.A.; Cruz-Mejía, H.; Flores-Garcia, N.S.; Porcayo-Calderon, J. Electrochemical Performance of Fe40Al-X (X = Cr, Ti, Co, Ni) Alloys Exposed to Artificial Saliva. Materials 2020, 13, 1095
TECNOLOGÍA DE LA CORROSIÓN
Versión publicada
publishedVersion - Versión publicada
Aparece en las colecciones: Artículos Publicados en Revistas Indexadas

Cargar archivos:


Fichero Tamaño Formato  
Electrochemical performance of Fe40Al-X.pdf3.1 MBAdobe PDFVisualizar/Abrir